(For beginner) Plywood knowledge& Manufacturing Experience Part 80: HOW MUCH TIME OF THE COLD PRESSING FOR YOUR HPL PLYWOOD ?

CHecked with many factories,in the summer season hot and dry temperature ,normally make more than 6 hours cold pressing time after laminating the HPL sheets on the substrate . Some mills also less 6 hours ,can you guess the quality of the HPL plywood and all the cold pressing time …

Read More »

(For beginner) Wood Face veneer knowledge & Manufacturing Exaperience Part 2: THICK NATURAL/RED/WHITE BIRCH FACE VENEER 0.35MM TO 0.50MM FOR HIGH QUALITY BIRCH PLYWOOD

Thick natural/red/white birch face veneer 0.35mm to 0.50mm for high quality birch plywood The face veneer mill is located in zhubao ,closed to the G237 road ,closed to zhongyi and anshui plywood mill . The boss is Mr.Sun,they only produced high quality birch B to E ,only thick face veneer …