China Plywood ,wood face veneer lamination conditioning time ?

If white birch ,normally before the hot pressing ,after glue spraying ,Minimum 2 hours conditioning time that would be better ,can maximum reduce the potential risks of telegraphing and bleeding .

If Okoume or other Bingtangor face veneer ,maybe the time can be changed ..

So ,when visit factories check their regular production time and see how to improve the quality and production .From their production management ,we can know their final quality of the their plywood .

Substrate Coverage agent Spraying 

24 hours conditioning

Substrate/Platform Gluing 

2 hours conditioning 

Face veneer platform Cold Pressing  

20 to 40 Minutes conditioning 

Face veneer platform hot pressing 

 

 

 

 