5-Ply ,7-Ply thick core veneer plywood Inspection and QC checklist

5-Ply ,7-Ply thick core veneer plywood Inspection and QC checklist

THick core veneer plywood in China ,it is hard to produce ,because of the limited log diameter ,hard to peel thick core veneer ,when producing the thick core veneer plywood ,need selected good core veneer .

Now ,in order to reduce the formaldehyde emission ,most of the thick core veneer plywood are used for melamine plywood in China .Also some foreign buyers use this thick core veneer plywood to make platforms and lamination .

In China ,normally 18mm have 9 plies ,11 plies and 13 plies ,this is standard core veneer thickness and quantity .But if produce 5 plies or 7 plies ,first is thick core veneer ,second is the core voids and overlaps are difficult to control .

1.Check the thick core veneer plywood core voids and overlaps

2.Scarf joint core veneer can avoid the overlaps and core voids

3.Straight core veneer ,no missing core veneer

So ,when inspect the thick core veneer plywood ,should be very careful .

If produce oversize or jumbo size plywood ,it is still hard to produce .

如无特殊说明,文章均为本站原创,转载请注明出处。If there are no special instructions, the articles are original, if you want to use or reproduce, please indicate the original source www.plywoodinspection.com

Check Also

Small Stories in Plywood Quality Control Industry Part 5

Small Stories in Plywood Quality Control Industry Part 5 The True Story of Quality Control …

Leave a Reply

Your email address will not be published. Required fields are marked *