Determination of Plywood Bonding Strength by Boiling Test part 6 

Determination of Plywood Bonding Strength by Boiling Test part 6

Class IV plywood: Dry test was carried out on specimens with water content meeting the requirements. Note: Water content of specimen should be controlled between 8% and 12%.

如无特殊说明,文章均为本站原创,转载请注明出处。If there are no special instructions, the articles are original, if you want to use or reproduce, please indicate the original source www.plywoodinspection.com,If you find that our articles infringe on your copyrights and interests, please email us at info@plywoodinspection.com in time and we will delete it at the first time.