Difference between phenolic glue and Melamine glue building formwork film faced plywood

Difference between phenolic glue and Melamine glue building formwork film faced plywood

In the daily construction, the most commonly used phenolic resin building formwork and melamine  film faced plywood rubber building formwork, then what is the difference between the two?

1. Quality: Phenolic glue building formwork  film faced plywood is better than melamine glue building formwork film faced plywood.

2. Use times: Phenolic glue board can be turned over more than 25 times, and melamine glue film faced plywood can be turned over more than 10 times.

3. Waterproofing performance: Phenolic resin film faced plywood building formwork is better than ordinary building formwork film faced plywood in waterproofing performance, and the price of building formwork is also higher than that of melamine glue.

4. Experimental Cementing Degree: Phenolic film faced plywood boiled in boiling water for 24 hours without glue, Melamine glue  film faced plywood boiled in boiling water for 5 hours without delamination.

如无特殊说明,文章均为本站原创,转载请注明出处。If there are no special instructions, the articles are original, if you want to use or reproduce, please indicate the original source www.plywoodinspection.com,If you find that our articles infringe on your copyrights and interests, please email us at info@plywoodinspection.com in time and we will delete it at the first time.

Check Also

F14 Structural Form Ply Inspection,grading,quality control,sourcing ,manufacturing

    Premium Form F14 Structural Form Ply – achieve concrete forming that results in …

Leave a Reply

Your email address will not be published. Required fields are marked *