FILM FACED PLYWOOD Production Process Flow

inspection rules and tips:film faced plywood production process
inspection rules and tips:film faced plywood production process

1. VENEER DRYING
Natural veneer usually has moisture content from 35-45%. Veneer drying will improve product characteristics making it more sturdy and resistant to high humidity, pressure, and harsh environment.

2. VENEER LAY-UP
After veneer is dried to favored moisture content, they are laid up perpendicularly by layer.

3. COLD PRESSING
Cold pressing ensures product structure before the permanent hot pressing.

4. HOT PRESSING
Hot Pressing permanently cures WBP Glue to solidify product structure.

5. SANDING AND CUTTING
After product surface is sanded, plywood is trimmed to specific dimensions.

6. FILM LAMINATING
Plywood is laminated with Phenolic Film Layer to resist moisture and maintain high- quality flat concrete surface.

7. EDGE TREATMENT
Plywood edges are then treated with oil-based/epoxy paint to resist envi- ronment humidity.

8. PRODUCT PACKAGING
Products are packaged and stored in a dry and controlled environment.

9. SHIPPING
Products are delivered to construction sites based on customers’ orders and schedules.

10. AT CONSTRUCTION SITE
VINAWOOD Film Faced plywood makes flat and high-quality concrete surface.

Special thanks to the original source of https://vinawoodltd.com/products/film-faced-plywood/production-process/

如无特殊说明,文章均为本站原创,转载请注明出处。If there are no special instructions, the articles are original, if you want to use or reproduce, please indicate the original source www.plywoodinspection.com,If you find that our article infringes on your rights and interests, please email us in time and we will delete it at the first time.

Check Also

Wire Mesh Anti-slip Film Faced Plywood Manufacturing defects

Wire Mesh Anti-slip Film Faced Plywood Manufacturing defects,catalog of film faced plywood grades,Quality Control Of …

Leave a Reply

Your email address will not be published. Required fields are marked *