Main factors affecting the quality of three-layer solid wood composite floor

Main factors affecting the quality of three-layer solid wood composite floor

The main factors affecting the quality of three-layer solid wood composite floor are as follows:

1. The moisture content of the laminate; the moisture content of the three-layer solid wood composite floor directly affects the quality of the floor. In order to ensure the dimensional stability of the three-layer solid wood composite floor in the use process (explanation: stable and stable; no change), the moisture content of the whole floor must be uniform inside and outside (J ū N Y ū n), without the phenomenon of external dry and internal wet. How much does the whole cabinet cost to ensure that the edge is sealed tightly, the lines are smooth, and all kinds of convenient and fashionable hardware are equipped. The ingenious combination endows the home with more humanized ideas and makes our room space more harmonious and comfortable. The surface, core and base plate of three-layer solid wood composite floor must be dried, and the moisture content of the surface and core plate is 6% – 8%, and the base plate is 5% – 7%.

5a1bd44acabaa1471.jpg

2. Paint quality; the quality of the paint surface determines the beauty and practicability of the floor in the use process. How much is the total wardrobe customization? The wardrobe customization has become an essential part of modern family decoration. Customized wardrobe, due to its customization, environmental protection, fashion, professional and other characteristics, is destined to become the consumption hotspot of family wardrobe in the next few years. The paint surface can be divided into roll (g ǔ n) paint, spray paint and roll paint according to the quality. The surface of three-layer solid wood composite floor is usually painted with phenol UV drying paint, three coats of primer and two coats of finish paint; the amount of paint is not less than 60g / m2, most of which are roller (g ǔ n) paint process, and there is absolutely no paint at the groove of four sides.

3. The adhesive quality of three-layer solid wood composite floor is formed by hot pressing three-layer boards with different thickness. Therefore, the quality of the adhesive directly affects the quality of three-layer solid wood composite floor. In the production process, the enterprise should adopt the adhesive with good waterproof performance, high strength, good aging resistance and low free formaldehyde content High quality adhesive. How much does the whole cabinet cost? What is the technological level of a cabinet? Edge sealing is extremely important. Manual edge sealing is neither strict nor neat. The factory production greatly improves and improves the precision and technological level of workmanship in terms of production. In terms of production cycle, it also greatly shortens the time. All processes are completed in one breath in the factory, and can be completed in a short time after installation on site Cheng.

4. Strict process management; the production of three-layer solid wood composite floor has strong technology and high processing accuracy. Therefore, the quality must be strictly controlled in each process

如无特殊说明,文章均为本站原创,转载请注明出处。If there are no special instructions, the articles are original, if you want to use or reproduce, please indicate the original source www.plywoodinspection.com,If you find that our articles infringe on your copyrights and interests, please email us at info@plywoodinspection.com in time and we will delete it at the first time.

Check Also

The common quality problems of solid wood floor

The common quality problems of solid wood floor are as follows: (1) noise The main …

Leave a Reply

Your email address will not be published. Required fields are marked *