Plywood Glue adhesive : Things you may not know about Melamine Glue

Plywood Glue adhesive : Things you may not know about Melamine Glue

Lower quality melamine plywood can sustain 4-8 hours boiling without delaminating. Higher end melamine can last between 10-20 hours in the boil test.

如无特殊说明,文章均为本站原创,转载请注明出处。If there are no special instructions, the articles are original, if you want to use or reproduce, please indicate the original source www.plywoodinspection.com,If you find that our articles infringe on your copyrights and interests, please email us at info@plywoodinspection.com in time and we will delete it at the first time.