Quality Standard for Fine Sand Procedure of Blockboard

Quality Standard for Fine Sand Procedure of Blockboard

Fine Sand Procedure

I. Quality Standards:

1. After fine sand, the surface of the board is smooth and smooth. 2. There is no sand penetration or other damage on the surface of the board. A kind of

3. After sanding, according to the requirements: 1.5 board 90 pieces for a stack, 1.6 board 80 pieces for a stack, 1.8 board 70 pieces for a stack, and neatly stacked.

如无特殊说明,文章均为本站原创,转载请注明出处。If there are no special instructions, the articles are original, if you want to use or reproduce, please indicate the original source www.plywoodinspection.com,If you find that our articles infringe on your copyrights and interests, please email us at info@plywoodinspection.com in time and we will delete it at the first time.

Check Also

pLYWOOD processing inspection,quality control ,sourcing and testing

pLYWOOD processing inspection,quality control ,sourcing and testing Cutting-to-size CNC-machining Edge machining Decorative finishing Special overlaying …

Leave a Reply

Your email address will not be published. Required fields are marked *