SVEZA Film Faced Birch Plywood Catalogs of plywood grades Defects Part 1 :Burnt film(burnouts) due to face veneer defects : coarse peeling

SVEZA Film Faced Birch Plywood Catalogs of plywood grades Defects Part 1 :Burnt film(burnouts) due to face veneer defects : coarse peeling

Special thanks to the original source of http://baza.sveza.ru/eng/index.php?pid=2&pr=1

Burnt film (burnouts) due to face veneer defects: coarse peeling

Bk

Burnt film (burnouts): film damage in the surface indents resulting from local wood removal during processing.

Measured by the length and the width of the area occupied, expressed as a percentage of the total sheet area.
coarse peeling
coarse peeling