Mechanical defects (pinholes, saw cuts)

Back

Pinhole is a local damage by a sharp object.

Saw cut is a local damage done during raw material cutting.

Tear-out is a hollow on the surface as a result of local tear-out of grain during processing.

Pinholes are measured at the maximum diameter.
Mechanical defects (pinholes, saw cuts)
Mechanical defects (pinholes, saw cuts)
如无特殊说明,文章均为本站原创,转载请注明出处。If there are no special instructions, the articles are original, if you want to use or reproduce, please indicate the original source www.plywoodinspection.com,If you find that our article infringes on your rights and interests, please email us in time and we will delete it at the first time.

Check Also

British Standard 1088 (Joubert Okoume & Hydrotek Marine Meranti) GRADING RULES

British Standard 1088 (Joubert Okoume & Hydrotek Marine Meranti) GRADING RULES B.S. 1088 : 1966 …

Leave a Reply

Your email address will not be published. Required fields are marked *