SVEZA Interior and Exterior Plywood grades Defects Part 25:Pasted veneer chips

SVEZA Interior and Exterior Plywood grades Defects Part 25:Pasted veneer chips

Pasted veneer chips are glued-in or pressed-in veneer inserts.

Pasted chips are measured by length and width
Pasted veneer chips
Pasted veneer chips

http://baza.sveza.ru/eng/index.php?pid=2&pr=2&id=39&def_id=39&full=1

如无特殊说明,文章均为本站原创,转载请注明出处。If there are no special instructions, the articles are original, if you want to use or reproduce, please indicate the original source www.plywoodinspection.com,If you find that our articles infringe on your copyrights and interests, please email us at info@plywoodinspection.com in time and we will delete it at the first time.