WBP Plywood Technical Information

Technical Information (WBP Plywood)

Technical Characteristics (Average)    
Property Unit Mean Value Test Method BSI Standard Reference
Bonding Quality Pretreatment 5.1.1 N/mm2 1.17~1.92 Immersion 24 hours in water 20oC & Pull Test  EN314-1:1993
Apparent Wood Failure % 25
Pretreatment 5.1.4 N/mm2 1.00~1.43 Immersion 72 hours in boiling water 100oC & Pull Test EN314-2:1993

 

Apparent Wood Failure % 40
Bending Strength / Modulus of Elasticity Lateral N/mm2 37 Push Test EN310:1993
Longitudinal N/mm2 52
Lateral N/mm2 4625
Longitudinal N/mm2 6043
Density kg/m3 592 Weighing EN323:1993
Moisture content % 6~9 Weighing EN322:199

* The information published in this section is an overview of the products and sizes .  Please contact us directly for specific requests.

如无特殊说明,文章均为本站原创,转载请注明出处。If there are no special instructions, the articles are original, if you want to use or reproduce, please indicate the original source www.plywoodinspection.com,If you find that our articles infringe on your copyrights and interests, please email us at info@plywoodinspection.com in time and we will delete it at the first time.

Check Also

CNC machining inspection,quality control ,sourcing and testing

CNC machining   High quality CNC-machining Milling, manufacture of various elements, even ellipses, polygons, ovals Drilling …

Leave a Reply

Your email address will not be published. Required fields are marked *