1. Basic Information
Item | Details |
---|
Product Name | Pine Wood Molding (Various Profiles) |
Inspection Date | [DD/MM/YYYY] |
Batch No. | [Batch Number] |
Manufacturer | [Company Name] |
Inspection Standard | ISO 9001, ASTM D3737, EN 14220 |
2. Raw Materials & Certifications
Material | Certification/Standard | Remarks |
---|
Pine Wood (Pinus spp.) | FSC/PEFC Certified | Sustainable Sourcing |
Adhesives | CARB Phase 2, EPA TSCA Compliant | Low Formaldehyde Emission |
Coatings (Varnish/Stain) | EN 71-3 (Toy Safety), VOC-Free | Non-Toxic Finishes |
Preservatives | AWPA (U1 Standards) | Mold & Insect Resistance |
3. Common Defects (Visual & Processing)
Defect Type | Description | Acceptance Criteria |
---|
Knots | Dark, loose, or dead knots | ≤3mm, max 2 per 1m length |
Splits/Cracks | Longitudinal wood fiber separation | Not deeper than 1/3 thickness |
Warping | Twisting, bowing, or cupping | ≤2mm deviation over 1m length |
Surface Roughness | Uneven sanding or machining marks | Smooth, no visible tool marks |
Glue Residue | Excess adhesive on edges/surface | No visible residue |
Color Variation | Inconsistent staining/finishing | Within approved sample range |
4. Laboratory Test Data (Performance & Functional Tests)
Test Item | Standard | Requirement | Test Result |
---|
Moisture Content (%) | ASTM D4442 | 8%-12% | 10.2% |
Density (kg/m³) | ISO 3131 | 400-600 kg/m³ | 480 kg/m³ |
Bending Strength (MPa) | ASTM D143 | ≥50 MPa | 62 MPa |
Formaldehyde Emission | EN 717-1 (E1/E0) | ≤0.1 ppm (E0) | 0.05 ppm |
Paint Adhesion | ASTM D3359 | Class 4B (Cross-Cut) | Pass |
Abrasion Resistance | EN 438-2 | ≤0.08g/100 cycles | 0.06g |
5. Production Processes & Joinery Methods
Process | Description | Quality Control Check |
---|
Kiln Drying | Reduces moisture to 8-12% | Moisture meter verification |
Planer Milling | Shapes profiles (e.g., baseboard, crown) | CNC precision (±0.5mm tolerance) |
Finger Jointing | End-to-end splicing for long lengths | Glue line strength ≥ wood strength |
Sanding | 120-220 grit for smoothness | Visual & touch inspection |
Finishing | Staining/varnishing (spray/dip) | Even coating, no drips/bubbles |
Common Joinery Methods:
- Butt Joint (Simple end-to-end, glued/nailed)
- Miter Joint (45° angle cuts for corners)
- Spline Joint (Reinforced with a wooden strip)
- Tongue & Groove (Interlocking edges for stability)
Notes:
- All test results should comply with international standards (e.g., ANSI, EN, ISO).
- Rejected batches must be reworked or discarded based on defect severity.