Principles to minimise potential problems with Class 2 and Class 3 off form Surface Finishes,F17 FORMPLY TECHNICAL ,formwork plywood inspection,graders checklist, AS 6669 Plywood sourcing service,phenolic surface film Testing

Principles to minimise potential problems with Class2 and Class 3 off form Surface FinishesPrinciple One: Most issues with off form surface finishes are associated with moisture.Wherever possible protect the formwork from weather. This includestarping where practical.Principle Two: The phenolic surface film used on formwork plywood is not impermeableto moisture. To ensure that moisture penetration is minimised, releaseagent and form oils …