Read More »Veneer Core Delamination & Blistering in Birch Plywood: Classification, Root Causes & NDT Inspection (Including SEA Factory Operational Status) ,March 22nd,2026
I. Precise Classification (3 Core Dimensions, Universal for QC Filing) 1. By Defect Location (Easiest On-Site Identification) Core Interlayer Delamination/Blistering: Most common; separation at veneer-to-veneer bonding interface with varying areas Core-to-Face/Back Transition Layer Delamination: Critical stress-bearing zone, prone to extended cracking and structural strength reduction Local Spot Delamination: Small-area single-point hollowing, mostly isolated process flaws 2. By Visual Morphology (Visual …